Titanium and zirconium complexes 1-3 (1 = (t-BuOS)(2)Ti(O-i-Pr)(2); 2 = (t-BuOS)(2)Zr(O-t-Bu)(2); 3 = ((OS)-O-Cum)(2)Zr(O-t-Bu)(2)) supported by two phenolate bidentate ligands (t-BuOS-H = 4,6-di-tert-butyl-2-phenylsulfanylphenol and (OS)-O-Cum-H = 4,6-di-cumyl-2-phenylsulfanylphenol) promoted the copolymerization of L-lactide with epsilon-caprolactone. The reactivity displayed by the two monomers during the copolymerization experiments and the microstructure disclosed by C-13 NMR analysis indicated a gradient distribution of the two monomers along the polymer chain. Copolymers with high epsilon-caprolactone content showed a large scale formation of crystalline spherulites prone to perfection of the crystallinity upon thermal annealing at 50 degrees C. Differently L-lactide rich copolymers revealed a thin film morphology consisting of small rigid domains of L-lactide segments of about 15 nm embedded in a soft matrix of the counterpart. Copolymers with comparable mole fractions of the two monomers were entirely amorphous.

Poly(lactide-co-ε-caprolactone) copolymers prepared using bis-thioetherphenolate group 4 metal complexes: Synthesis, characterization and morphology

DELLA MONICA, FRANCESCO;
2014-01-01

Abstract

Titanium and zirconium complexes 1-3 (1 = (t-BuOS)(2)Ti(O-i-Pr)(2); 2 = (t-BuOS)(2)Zr(O-t-Bu)(2); 3 = ((OS)-O-Cum)(2)Zr(O-t-Bu)(2)) supported by two phenolate bidentate ligands (t-BuOS-H = 4,6-di-tert-butyl-2-phenylsulfanylphenol and (OS)-O-Cum-H = 4,6-di-cumyl-2-phenylsulfanylphenol) promoted the copolymerization of L-lactide with epsilon-caprolactone. The reactivity displayed by the two monomers during the copolymerization experiments and the microstructure disclosed by C-13 NMR analysis indicated a gradient distribution of the two monomers along the polymer chain. Copolymers with high epsilon-caprolactone content showed a large scale formation of crystalline spherulites prone to perfection of the crystallinity upon thermal annealing at 50 degrees C. Differently L-lactide rich copolymers revealed a thin film morphology consisting of small rigid domains of L-lactide segments of about 15 nm embedded in a soft matrix of the counterpart. Copolymers with comparable mole fractions of the two monomers were entirely amorphous.
2014
2014
http://pubs.rsc.org/en/journals/journalissues
Chemical Engineering (all); Chemistry (all)
DELLA MONICA, Francesco; Luciano, Ermanno; Buonerba, Antonio; Grassi, Alfonso; Milione, Stefano; Capacchione, Carmine
File in questo prodotto:
File Dimensione Formato  
RSC2014.pdf

non disponibili

Tipologia: Documento in Post-print
Licenza: DRM non definito
Dimensione 1.4 MB
Formato Adobe PDF
1.4 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11383/2129294
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 41
  • ???jsp.display-item.citation.isi??? 35
social impact